TECHNET Archives

November 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Post, Scott E" <[log in to unmask]>
Date:
Thu, 18 Nov 2010 13:16:36 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Neifer, Gebhard" <[log in to unmask]>
Subject:
From:
"Neifer, Gebhard" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (102 lines)
10% rule sounds to me like apperture size is typically 10% smaller than pad size, does that make sense?


Gebhard

-----Ursprüngliche Nachricht-----
Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Post, Scott E
Gesendet: Donnerstag, 18. November 2010 13:58
An: [log in to unmask]
Betreff: Re: [TN] Solder Paste Transfer Efficiency

You're right - those graphs you see of area ratio vs. transfer efficiency are averages and I don't find them very useful as area ratio shrinks.  As you mentioned, when the apertures get very small I prefer box plots and looking for outliers.  I also like to create xbar/R charts and look for stability and in control.  It's worthwhile to sub-group in various ways to understand where variation is coming from.  I typically subgroup by reference designator, by board, by squeegee direction (you'll be amazed at the difference between front-back & back-front).  With QFPs you can subgroup by aperture orientation (top/bottom vs. left/right) and see very large differences.  Sub-grouping by board can help you identify the best wipe frequency or the effect of abandon time.

I'm not sure what the "10% rule" is.

Scott Post
Staff Manufacturing Engineer
P.O.U. 0000-001E-0CTC
2151 E. Lincoln Road
Kokomo, Indiana    46904-9005
765-451-2983 (Phone)
765-451-0287 (FAX)

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gumpert, Ben
Sent: Thursday, November 18, 2010 7:45 AM
To: [log in to unmask]
Subject: [TN] Solder Paste Transfer Efficiency

Hey TechNetters,

I've got a couple questions for the solder paste printing gurus:

1. Can someone explain something about transfer efficiency for me? The typical chart (see below) shows a nice, clean set of points, but I know that my process has variation. So is transfer efficiency just about averages? The average volume printed for a specific aperture divided by the aperture volume? Meaning that instead of single points shown in the chart below, box plots would really be more accurate?

Transfer
Efficiency
100%     |                                                                    x             x
                |                                                    x
                |                                              x
                |                                            x
50%        |                                       x
                |                             x
                |            x
                |
0%          |_________________________________________________
                .3            .4            .5            .6            .7            .8            .9            1.0
                                                Area Ratio

2. What is the 10% rule? I've read a couple of articles that mention the 10% rule, but they don't make it clear what it is. I interpret it to mean that to have an 'acceptable' solder printing process, the standard deviation of the individual data points of paste printed (transfer efficiency) needs to be 10% or less of the average paste transferred. Am I on the right track here?

Thanks,
Ben


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
**************************************************************************************** Note: If the reader of this message is not the intended recipient, or an employee or agent responsible for delivering this message to the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify us immediately by replying to the message and deleting it from your computer. Thank you. ****************************************************************************************

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
**************************************************************************************** Note: If the reader of this message is not the intended recipient, or an employee or agent responsible for delivering this message to the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify us immediately by replying to the message and deleting it from your computer. Thank you. ****************************************************************************************

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2