TECHNET Archives

November 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 18 Nov 2010 08:14:33 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Subject:
From:
Joyce Koo <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (70 lines)
Your paste company should explain to you in details. If they don't, change paste company. 
--------------------------
Sent using BlackBerry


----- Original Message -----
From: Gumpert, Ben [mailto:[log in to unmask]]
Sent: Thursday, November 18, 2010 07:45 AM
To: [log in to unmask] <[log in to unmask]>
Subject: [TN] Solder Paste Transfer Efficiency

Hey TechNetters,

I've got a couple questions for the solder paste printing gurus:

1. Can someone explain something about transfer efficiency for me? The typical chart (see below) shows a nice, clean set of points, but I know that my process has variation. So is transfer efficiency just about averages? The average volume printed for a specific aperture divided by the aperture volume? Meaning that instead of single points shown in the chart below, box plots would really be more accurate?

Transfer
Efficiency
100%     |                                                                    x             x
                |                                                    x
                |                                              x
                |                                            x
50%        |                                       x
                |                             x
                |            x
                |
0%          |_________________________________________________
                .3            .4            .5            .6            .7            .8            .9            1.0
                                                Area Ratio

2. What is the 10% rule? I've read a couple of articles that mention the 10% rule, but they don't make it clear what it is. I interpret it to mean that to have an 'acceptable' solder printing process, the standard deviation of the individual data points of paste printed (transfer efficiency) needs to be 10% or less of the average paste transferred. Am I on the right track here?

Thanks,
Ben


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2