TECHNET Archives

November 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 24 Nov 2010 10:00:18 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Werner Engelmaier <[log in to unmask]>
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Content-Type:
text/plain; charset="utf-8"
In-Reply-To:
<6CA7DF04267F474097A9B082611AD1CB@dell3a3601fa11>
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (139 lines)
 Hi Inge,
Indeed, the 4% is a 'red flag' without much scientific validity—see attached columns.
There also was a Gerd Becker at Ericsson.
Werner

 


 

 

-----Original Message-----
From: Inge <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, Nov 24, 2010 5:56 am
Subject: Re: [TN] Ductile to Brittle transition


Werner, 
 
Thanks for the posting with declarations and illustrations of IMC impact on solder ductility etc. 
I'm not a chrystallography guy, nor a thermodynamic freak, so I need some further explanation. Have patience with me, please. At my age,  the brain is not so quick any longer. 
 
If one gradually increases the Au percentage in SnPb, the size and number of IMC platelets undergo a increase. The forbidden level is assumed to be when you pass 4 wt%.  Over that level you get to brittle solder joints.  That's clear. 
 
If one lowers the Lead content gradually, I've seen that the size and number of IMC platelets undergo a decrease until, finally, they vanish completely. With other words, if you have just Sn, you can increase the Au percentage until you get the much used 80AuSn. In this case you get an extremly fine grade, dense and IMC-free solder joint. How come that no AuSn IMCs are grown now? Is  the reason for IMC growth in SnPb that you have a binary situation? 
 
I'll send a diagram to Steve. An old one which I have been using for 20 years when speaking to colleagues.  Are the figures still actual  or do you use different data today?   From these graphs, I used to tell people, don't feel too safe about the 4wt% rule, things happen to the solder joint before that level. 
 
(The diagram is  from Dr Willy Beckers at Ericsson, retired since many years. He was our solder guru. There is none of his kind today at Ericsson) 
 
Inge 
 
PS. I forwarded  your excellent report to RUAG Space analysis lab. They found it to be a gold coffin of comprehension. 
 
 
----- Original Message ----- From: "Inge" <[log in to unmask]> 
To: <[log in to unmask]> 
Sent: Wednesday, November 24, 2010 12:01 AM 
Subject: Re: [TN] Ductile to Brittle transition 
 
> In fig 14 and 15 you say that IMCs are sticking out , and as I can see it, > they are needles. 
> 
> Inge 
> 
> 
> 
> 
> Hi Inge, 
> 1. Not a good simile—the steel in concrete only adds strength in tension, > not compression, it is not brittle, and it is round; IMCs are NOT > needles—they only appear that way when the platelets are sectioned at > acute angles; the adhesion of the concrete to steel is very high, not so > solder to IMC. 
> 2. Crystal growth at times appears [at least] chaotic. 
> 3. I think it is the basic material properties—similar to all crystal > structure—high modulus and little ductility. 
> 4. Certainly the presence of the constituent metals is required—Margareta > Nylen in Sweden has shown that when all the Sn was used up in forming > IMCs, no more dissolution took place—elegant experiment; solidification > speed certainly would have an impact, I would think impurities as well. 
> Skoal, 
> Werner 
> 
> 
> 
> 
> 
> 
> ----- Original Message ----- > From: "Inge" <[log in to unmask]> 
> To: <[log in to unmask]> 
> Sent: Tuesday, November 23, 2010 10:28 PM 
> Subject: [TN] Ductile to Brittle transition 
> 
> 
>> Hi, 
>> have a few questions on Konstantina's and your report. 
>> 
>> 1.  If you place steel bars or steel nets in the concrete, the strength >> will increase significantly, but the IMC plates and needles in the >> sollder joint do the opposite. How com? 
>> 
>> 2. Why are so many geometries created? Large plates, small plates, >> needles, bars, all in a chaotic oder. 
>> 
>> 3.  What causes the predominant brittleness, size of IMCs or geometric >> form or  anything else? 
>> 
>> 4. What is the major driving force to build up the IMC structure, >> percentage of xx in the solder, or solidification speed or what? 
>> 
>> Inge 
>> 
>> ______________________________________________________________________ 
>> This email has been scanned by the MessageLabs Email Security System. 
>> For more information please contact helpdesk at x2960 or [log in to unmask] >> ______________________________________________________________________ 
>> 
>> --------------------------------------------------- 
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0 
>> To unsubscribe, send a message to [log in to unmask] with following text in 
>> the BODY (NOT the subject field): SIGNOFF Technet 
>> To temporarily halt or (re-start) delivery of Technet send e-mail to >> [log in to unmask]: SET Technet NOMAIL or (MAIL) 
>> To receive ONE mailing per day of all the posts: send e-mail to >> [log in to unmask]: SET Technet Digest 
>> Search the archives of previous posts at: >> http://listserv.ipc.org/archives 
>> Please visit IPC web site >> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional >> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 >> ext.2815 
>> ----------------------------------------------------- > 
> 
> ______________________________________________________________________ 
> This email has been scanned by the MessageLabs Email Security System. 
> For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ 
> 
> --------------------------------------------------- 
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 
> To unsubscribe, send a message to [log in to unmask] with following text in 
> the BODY (NOT the subject field): SIGNOFF Technet 
> To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) 
> To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest 
> Search the archives of previous posts at: http://listserv.ipc.org/archives 
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 
> -----------------------------------------------------  
______________________________________________________________________ 
This email has been scanned by the MessageLabs Email Security System. 
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ 
 
--------------------------------------------------- 
Technet Mail List provided as a service by IPC using LISTSERV 15.0 
To unsubscribe, send a message to [log in to unmask] with following text in 
the BODY (NOT the subject field): SIGNOFF Technet 
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) 
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest 
Search the archives of previous posts at: http://listserv.ipc.org/archives 
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 
----------------------------------------------------- 

 

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2