Hi Jerry
To the best of my knowledge, you will get the same performances from a "standard" acrylic coating at a fraction of the cost. Keep-in-mind that the solvent is designed to go away leaving the coating behind.
Other fluorochemical coatings actually contain no polymer and we found - in my previous life - that when exposed to a temperature above 50DegC it volatilised off the assembly leaving no coating behind - it also came off on your fingers or any other surface it touched. We did not develop that into a saleable product!
Hope this helps
Graham Naisbitt
On 11 Aug 2010, at 15:06, Jerry Dengler wrote:
> Hello all,
>
>
>
> We have a request from a potential customer to use this 3M coating on
> their PCBA's. I do not have any experience with this one and wanted to
> see if any of you have used it. If so what did/do you think of it. I
> have used several different Humiseal products (1C49, 1B31, 1B73, 1A27)
> in the past so how does it compare.
>
>
>
> Thanks,
>
>
>
> Jerry Dengler
>
> Production Manager
>
> Pergamon Corporation
> 380 Crooked Lane, Unit# 3
> King of Prussia, PA 19406-2567
> U.S.A.
> (610) 239-0721 Phone
> (610) 239-0720 Fax
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|