Well, we have never used it here. A quick check shows that this material
is not on QPL-46058 so you would have a tough time putting it on military
or Class 3 hardware.
Doug Pauls
Jerry Dengler <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
08/11/2010 09:06 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Jerry Dengler <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] 3M Novec EGC-2702 Electronic Coating
Hello all,
We have a request from a potential customer to use this 3M coating on
their PCBA's. I do not have any experience with this one and wanted to
see if any of you have used it. If so what did/do you think of it. I
have used several different Humiseal products (1C49, 1B31, 1B73, 1A27)
in the past so how does it compare.
Thanks,
Jerry Dengler
Production Manager
Pergamon Corporation
380 Crooked Lane, Unit# 3
King of Prussia, PA 19406-2567
U.S.A.
(610) 239-0721 Phone
(610) 239-0720 Fax
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|