Yep.
I used to use it for sticking patch antennas onto aircraft fuselages.
Good stuff, provided you don't want to take the components apart again.
Ever.
On 10/06/2010 17:17, Ken Bloomquist wrote:
> While I've never used it for bonding wires to a board 3M VHB (Very High
> Bond) double backed tape holds like crazy. I use it for anything automotive
> where I don't want to drill any holes but want it to stay on forever. It's
> the same tape that auto manufacturers use to attach name placards and much
> more.
>
> KennyB
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Linda Langley
> Sent: Thursday, June 10, 2010 9:08 AM
> To: [log in to unmask]
> Subject: [TN] double sided tape
>
> Does anyone know of a company that makes a double sided tape I could use
> to secure wires to the bottom of a board? I have used the Tape Dots
> from Circuit Medic and they work great but now I need double sided
> adhesive.
>
>
>
> Any help will be greatly appreciated!!!!!
>
>
>
> Linda Langley CIT
>
> Training Specialist
>
> Jabil Circuit
>
> 248-292-6176
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
--
Eric Christison Msc
Mechanical Engineer
Consumer& Micro group
Imaging Division
STMicroelectronics (R&D) Ltd
33 Pinkhill
Edinburgh EH12 7BF
United Kingdom
Tel: +44 (0)131 336 6165
Fax: + 44 (0)131 336 6001
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|