Yep. I used to use it for sticking patch antennas onto aircraft fuselages. Good stuff, provided you don't want to take the components apart again. Ever. On 10/06/2010 17:17, Ken Bloomquist wrote: > While I've never used it for bonding wires to a board 3M VHB (Very High > Bond) double backed tape holds like crazy. I use it for anything automotive > where I don't want to drill any holes but want it to stay on forever. It's > the same tape that auto manufacturers use to attach name placards and much > more. > > KennyB > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Linda Langley > Sent: Thursday, June 10, 2010 9:08 AM > To: [log in to unmask] > Subject: [TN] double sided tape > > Does anyone know of a company that makes a double sided tape I could use > to secure wires to the bottom of a board? I have used the Tape Dots > from Circuit Medic and they work great but now I need double sided > adhesive. > > > > Any help will be greatly appreciated!!!!! > > > > Linda Langley CIT > > Training Specialist > > Jabil Circuit > > 248-292-6176 > > > ______________________________________________________________________ > This email has been scanned by the MessageLabs Email Security System. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > > > ______________________________________________________________________ > This email has been scanned by the MessageLabs Email Security System. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > > -- Eric Christison Msc Mechanical Engineer Consumer& Micro group Imaging Division STMicroelectronics (R&D) Ltd 33 Pinkhill Edinburgh EH12 7BF United Kingdom Tel: +44 (0)131 336 6165 Fax: + 44 (0)131 336 6001 ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------