TECHNET Archives

June 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="utf-8"
X-To:
Date:
Thu, 17 Jun 2010 12:57:21 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Chris Mahanna <[log in to unmask]>
Subject:
From:
Chris Mahanna <[log in to unmask]>
MIME-Version:
1.0
Content-Transfer-Encoding:
base64
Sender:
Parts/Attachments:
text/plain (1 lines)
So we’ve got a new toy, and now can image SJ failures a little differently.  Requesting all experts to help me speak more intelligently about what we see.  (until AJ-820 is published ☺)

These are of major interest to me today.  It’s the easy stuff.  It’s the weak link. It’s thru hole.  As always, I may or may not know the history.  As an independent lab, our customers don’t usually tell us much.  I suppose they’re fearful that we may just regurgitate.

http://ipc-technet.groupsite.com/gallery/13892

Chris

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2