Hi Karen,
IPC 1-10c has drafted 2221 appendix A as the new and improved system for conformance coupons. In the draft, the M coupon has been dumped and in its place is the new "W" coupon. The "W" coupon includes features for dip-n-look, NPL-SMART-Bob Willis et. al. Spread, and wetting balance.
Underway currently are project(s) to correlate Spread to Wetting Balance parametric pass/fail, which implies that in the near future we should be able to move Spread and Wetting Balance to J-STD section for test with pass/fail!
I hesitate to so publicly announce such activities, but I have a vested (volunteer) interest in no surprise dissention during 1-10c voting in September.
I'll contact you offline with the information on how to get the draft gerbers for W.
Chris
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Karen Tellefsen
Sent: Wednesday, June 30, 2010 10:14 AM
To: [log in to unmask]
Subject: [TN] wetting coupon J-STD-003B
Does anyone know where I can get the wetting coupon shown in Figure 4-3 of
J-STD-003B
Karen Tellefsen - Electrical Testing
[log in to unmask]
908-791-3069
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|