Hi Mordechai,
I would not worry too much about side fillets--the heel fillets are much more important.
What should be your real concern about the reliability of your TSOPs SJs is whether your TSOP leadframe is made of Alloy 42 instead of copper. That is where your reliability concern needs to be because of the large CTE-mismatch with FR-4.
Werner
-----Original Message-----
From: Mordechai Kirshenbaum <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, May 4, 2010 7:43 am
Subject: [TN] Minimum Side Joint Length
We have to assemble TSOP packages on SSOP foot print PCB. (The TSOP
package width is 40 mils shorter than the SSOP package width).
We found that the theoretical ( calculated) side joint length (D) will be in
some
instances less than the minimum acceptable side joint (as by IPC-A-610,
#8.2.5.4). (The available pad length on the PCB under the component lead is
less than the foot length).
It may be even worse if we have a slight solder defect, or if the component is
placed several mils off side.
What is the reliability impact?
Do you know about accelerated reliability tests or field data that show the
correlation between the failure rate and the side joint length?
Thankfully,
Mordechai Kirshenbaum
QA Team Manager
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|