Subject: | |
From: | |
Reply To: | |
Date: | Wed, 24 Mar 2010 14:17:03 -0300 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Hi Ioan
Well, it depends(tm).
Some shrink tubing has an adhesive layer inside it, to make it waterproof. This is what is used, for example, on the wiring for a pump that gets dropped down a well. If the shrink tubing used for these has that layer you are probably OK.
Is there any visible p/n on the shrink tubing? And/or at the exposed edge of the tube is there any visible adhesive, usually there will be squeeze-out at the ends.
If it's the non-adhesive stuff, then the answer is no...
regards,
- Graham
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Wednesday, March 24, 2010 1:02 PM
To: [log in to unmask]
Subject: [TN] Cable wash
Dear Technos,
Could I say that shrink tubing is water proof?
Otherwise said, I have this coax cable (connector - cable - connector) which has shrink tubing over both cable-connector junctions and wonder if it could pass through our in-line washer. What mainly bugs me is one of the connectors has a square body and with all those edges and corners I wonder how tight the tube can shrink around it. What I dread is not only water could seep under the tubing, but this could be dirty, ionic active water.
Thanks,
Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
T | 450.967.7100 ext.244
E | [log in to unmask] <mailto:[log in to unmask]>
W | www.digico.cc <http://www.digico.cc/>
N'imprimer que si nécessaire - Print only if you must
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|