TECHNET Archives

December 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 1 Dec 2009 12:16:54 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Chris Mahanna <[log in to unmask]>
Subject:
From:
Chris Mahanna <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (19 lines)
Sorry all.  I used the IAu subject line for thread following.
To recap:  We supposedly have IAu and hard Au on the same board.  I was led to believe (by the equipment manufacturer) that nano-identation would be a cost effective way to prove this.  It MAY be possible, but not with my sample.
SEM-EDS was part of the project (Phosphorous came in at 7%).  The EDS seemed to be working at low levels (it picked up trace Gallium from a FIB cut).
But we didn't find any Cobalt in the contact area, which was unexpected...

It has been quite a learning experience for me.  Thanks for the excellent feedback.  I believe the moral to the story is:  you better trust your offshore fab, because to prove out IPC-4552 and MIL-G-45204 conformance from a completed product is likely cost prohibitive.

Chris

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2