TECHNET Archives

December 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Chris Mahanna <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 3 Dec 2009 12:53:50 +0530
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Anil kher <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
From:
Anil kher <[log in to unmask]>
Parts/Attachments:
text/plain (47 lines)
Dear Chris

To identify Imm Au and Electrolytic Au - thickness may be the way. Imm Au
will not cross 0.08 to 0.1 um. Hard Gold may be higher if specified.
If both are specified in same range of 0.1 um - it will be difficult to
identify.

I do not believe they will perform differently also - at 0.1um. Except Imm
Au - badly done will give you solderability issues.

Anil

-----Original Message-----
From: Chris Mahanna [mailto:[log in to unmask]] 
Sent: Wednesday, December 02, 2009 21:31
Subject: Re: IAu hardness

Ah.  Joyce, thank you.  I think I should have ask: how common is Ni hardened
Au?
I may have misunderstood it to be rarely used in electronics.  My
metallurgist mentor retired 3 years ago.  We miss him.
Chris

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2