TECHNET Archives

December 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Lee Whiteman <[log in to unmask]>, TechNet <[log in to unmask]>
Date:
Tue, 8 Dec 2009 13:42:25 +0000
Reply-To:
Subject:
Content-Transfer-Encoding:
base64
MIME-Version:
1.0
Content-Type:
text/plain
From:
vladimir Igoshev <[log in to unmask]>
Parts/Attachments:
text/plain (1 lines)
Lee,



If both of the alloys will mix thoroughly during re-flow, it shouldn't make much of a difference whether you solder SAC balls with the eutectic paste, or vise versa.



Regards,



Vladimir





------Original Message------

From: Lee Whiteman

Sender: TechNet

To: [log in to unmask]

Subject: [TN] SnPb SOLDER BALLS WITH SAC SOLDER PASTE

Sent: Dec 8, 2009 08:17



I know about the problems with soldering BGAs with SAC solder balls and SnPb solder paste and read plenty of papers pro and con.



I heard about a report where if you solder BGAs with SnPb solder balls using SAC solder paste, the resulting solder joint will be unreliable. Has anyone heard of anything like that? If there are any cross-sections or papers that you can share with me, that would be great.



Thanks again.



Lee Whiteman, PMP

Senior Member Engineering Staff

L-3 Communications East

Telephone: (856) 338-3508

FAX: (856) 338-2906

E-Mail: [log in to unmask]

 









SENTEC

11 Canadian Road, Unit 7.

Scarborough, ON M1R 5G1

Tel: (416) 899-1882

Fax: (905) 882-8812

www.sentec.ca