Lee,
If both of the alloys will mix thoroughly during re-flow, it shouldn't make much of a difference whether you solder SAC balls with the eutectic paste, or vise versa.
Regards,
Vladimir
------Original Message------
From: Lee Whiteman
Sender: TechNet
To: [log in to unmask]
Subject: [TN] SnPb SOLDER BALLS WITH SAC SOLDER PASTE
Sent: Dec 8, 2009 08:17
I know about the problems with soldering BGAs with SAC solder balls and SnPb solder paste and read plenty of papers pro and con.
I heard about a report where if you solder BGAs with SnPb solder balls using SAC solder paste, the resulting solder joint will be unreliable. Has anyone heard of anything like that? If there are any cross-sections or papers that you can share with me, that would be great.
Thanks again.
Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]