When you find the solder ball is in the middle of the space, you shouldn't consider electrical clearance issue. It is 100% defect because the ball can move!
Best Regards,
James Liu 刘春光
Director, Technology & Standardization 技术与标准总监
IPC China
上海市长宁区延安西路1088号2303室
Suite 2303,#1088 West Yan'an Rd., Changning, Shanghai 200052 PRC
Tel: +86 21 5497 3435
Fax: +86 21 5497 3437
MP: +86 136 0133 3491
[log in to unmask]
www.ipc.org.cn
________________________________________
发件人: TGAsia [[log in to unmask]] 代表 Jackson Chan [[log in to unmask]]
发送时间: 2009年12月17日 11:53
收件人: Listserv TGAsia
主题: Re: [TGAsia] SMT reflow - microsolder ball requirement
Hi Alvin,
Thank you for your response.
I also read this table in IPC-610D before. You think that we should use
0.13mm (minimum electrical conductor spacing) to define minimum electrical
clearance stated in the solder ball requirement per clause 5.2.6.1 of
IPC-A-610D. Is that mean the solder ball should be located at least 0.13mm
distance from the pad of IC or have different meaning.
I raise one example - 0.5mm pitch IC and spacing between the pads of IC
lead is 0.22mm. The size of solder ball is 0.1mm.
If the solder ball is at the middle of space between the pads for lead, it
is impossible to have 0.13mm clearance from either side of IC pad. It also
implies that 0.5mm ptich , 0.4mm ptich or smaller pitch for IC does not
allow the presence of any solder ball . It seems that it is not so
feasible to have 100% "Pass" in every board.
Jackson
"Alvin(Suz)
Zhang(Suzhou)"
<Alvin-Suz.Zhang- To
[log in to unmask] "Jackson Chan"
nics.com> <[log in to unmask]>
cc
2009/12/17 上午 "Asia Committe Task Group Forum"
11:34 <[log in to unmask]>
Subject
RE: [TGAsia] SMT reflow -
microsolder ball requirement
Hi Jackson
Pls refer to this.
(Embedded image moved to file: pic09930.gif)
Best regards
Alvin Zhang
Supplier Development Engineering
Office No. : +86-512-67612300-8713
Mobile Phone No. : +86-13306209131
[log in to unmask] | www.flextronics.com | "Creating
value that increases customer competitiveness"
-----Original Message-----
From: Alvin(Suz) Zhang(Suzhou)
Sent: Thursday, December 17, 2009 11:28 AM
To: 'Jackson Chan'
Cc: 'Asia Committe Task Group Forum'
Subject: RE: [TGAsia] SMT reflow - microsolder ball requirement
Hi Jackson
The IPC have the definition of the min clearance , pls refer to IPC-610.
Best regards
Alvin Zhang
Supplier Development Engineering
Office No. : +86-512-67612300-8713
Mobile Phone No. : +86-13306209131
[log in to unmask] | www.flextronics.com | "Creating
value that increases customer competitiveness"
-----Original Message-----
From: TGAsia [mailto:[log in to unmask]] On Behalf Of Jackson Chan
Sent: Thursday, December 17, 2009 11:13 AM
To: [log in to unmask]
Subject: [TGAsia] SMT reflow - microsolder ball requirement
Dear all,
Recently, I have the discussion with the customer on the specification of
solder ball especially at the region between the leads of IC.
Referring to IPC-A-610D, section 5.2.6.1
It states that “solder balls do not violate minimum electrical clearance”
It came out the question on what is “minimum electrical clearance” and "how
to relate the solder ball (in terms of size and distance) to this minimum
electrical clearance"
IPC-2221 has the minimum electrical spacing under different voltage. For
typical voltage 0 - 15V, it is 0.13mm min. Should we use 0.13mm (minimum
electrical conductor spacing) to define minimum electrical clearance stated
in the solder ball requirement per clause 5.2.6.1 of IPC-A-610D ?
Hope IPC and experts here to elaborate the solder ball requirement here.
Regards,
Jackson
Legal Disclaimer: The information contained in this message may be
privileged and confidential. It is intended to be read only by the
individual or entity to whom it is addressed or by their designee. If the
reader of this message is not the intended recipient, you are on notice
that any distribution of this message, in any form, is strictly prohibited.
If you have received this message in error, please immediately notify the
sender and delete or destroy any copy of this message
|