The contact was designed for a low abrasion gold surface. Solder will abrade quite readily, or at least have the surface finish perturbed, when influenced by the installation of a sliding contact.
Interaction between a gold contact and a solder surface will not be stable over time. The gold will migrate into the solder.
Mike Green
Electronic Packaging Design
LMCO-Sunnyvale
408-743-1635
One Corporation, One Team
“If it was easy, they wouldn't call it rocket science.” M. Green, 2009
-----Original Message-----
From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of CJGlz_gwtc
Sent: Wednesday, December 09, 2009 4:20 PM
To: [log in to unmask]
Subject: Re: [IPC-600-6012] Gold Contacts with Solder Plated
My question is can they be used? What could be the potential problems, issues?
Constantino J. González, ACME, INC. - GALUSAMEX REPAIR Co.
President / Consultant Engineer - Official IPC MASTER INSTRUCTOR - IPC-A-610 Committee Chairman
USA Cell Phone: 605-381-5963 - Mexico Cell Phone: 55-2709 - 6392 - [log in to unmask] or [log in to unmask]
Skype - acmeinc_cjg
Does your Company need Rework, Repair or Inspection of Electronic Assemblies Services.
Do you have too much Rework, Scrap or Rejects from your Customer…..Call us, We can help!
GALUSAMEX REPAIR Co.
Please consider the environment before printing this email
This email communication may contain CONFIDENTIAL INFORMATION WHICH ALSO MAY BE LEGALLY PRIVILEGED and is intended only for the use of the intended recipients identified above. If you are not the intended recipient of this communication, you are hereby notified that any unauthorized review, use, dissemination, distribution, downloading, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify us by reply email, delete the communication and destroy all copies.
-----Original Message-----
From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of Gandhi, Mahendra S (AS)
Sent: Wednesday, December 09, 2009 3:51 PM
To: [log in to unmask]
Subject: Re: [IPC-600-6012] Gold Contacts with Solder Plated
Reject. Does not meet the drawing requirements (if I am not wrong).
Mahendra
-----Original Message-----
From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of CJGlz_gwtc
Sent: Wednesday, December 09, 2009 10:27 AM
To: [log in to unmask]
Subject: [IPC-600-6012] Gold Contacts with Solder Plated
Hello what could the possible impact that a PCB that it is supposed to have Gold Plated Contacts is with solder plated [Tin]. Can they be used. Any document that I can consult on the matter Please....
Constantino J. González, ACME, INC. - GALUSAMEX REPAIR Co.
President / Consultant Engineer - Official IPC MASTER INSTRUCTOR - IPC-A-610 Committee Chairman USA Cell Phone: 605-381-5963 - Mexico Cell Phone: 55-2709 - 6392 - <mailto:[log in to unmask]> [log in to unmask] or <mailto:[log in to unmask]> [log in to unmask] Skype - acmeinc_cjg Does your Company need Rework, Repair or Inspection of Electronic Assemblies Services.
Do you have too much Rework, Scrap or Rejects from your Customer.....Call us, We can help!
GALUSAMEX REPAIR Co.
image003 acme4
P Please consider the environment before printing this email
This email communication may contain CONFIDENTIAL INFORMATION WHICH ALSO MAY BE LEGALLY PRIVILEGED and is intended only for the use of the intended recipients identified above. If you are not the intended recipient of this communication, you are hereby notified that any unauthorized review, use, dissemination, distribution, downloading, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify us by reply email, delete the communication and destroy all copies.
,
SCORE=30 using global scores of TAG_LEVEL00.0
QUARANTINE_LEVEL=5 KILL_LEVEL=0
tests=D_RCVD_SINGLE
X-Barracuda-Start-Time: 1260404432
X-Barracuda-URL: http://10.10.10.49:8000/cgi-bin/mark.cgi
X-Barracuda-Virus-Scanned: by E-Filtering Spam Firewall at gwtc.net
X-Mailer: Microsoft Office Outlook 12.0
X-MessageGate-spam: 130
X-NAI-Spam-Report: 1 Rules triggered * 0 -- RV3424 -- BODY: Version number
X-NAI-Spam-Score: 0
X-Proofpoint-Spam-Details: rule=tspam policy�fault score=pamscore=pscore=hishscore
ulkscore
dultscore
lassifier=am adjust=eason=x e
|