TECHNET Archives

October 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steve Zweig <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Zweig <[log in to unmask]>
Date:
Wed, 7 Oct 2009 09:29:47 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (60 lines)
Hi Pete,

I just happen to notice your post.  As an x-ray manufacturer that supplies both top down and
angle viewing machines, I can tell you most opens are hard to detect with either.

You always hope to see a variation in grey scale on the x-ray image due to different density,
but this isn't always the case.

If you have a microcrack, a ball just sitting on a pad, a separate of the pad from the pc board,
the density will not have enough variation.  Unfortunately, this is the majority of opens.

I have an ERSASCOPE and a BGA-100 from SMT Tools in our lab.  I use it when I notice
an unusual ball shape on the x-ray image.  It's a good way to confirm the results.

The BGA-100 might be a good choice for you.  It's a handheld system that lets you do
a quick inspection.  The price is around $ 3,000.  We bought one for under $ 1,000.
You can ask them if they have specials.  I hope this helps.

Steve

________________________________________
From: TechNet [[log in to unmask]] On Behalf Of Pete Houwen [[log in to unmask]]
Sent: Wednesday, October 07, 2009 9:03 AM
To: [log in to unmask]
Subject: Re: [TN] BGA X-Ray Defect Detection Capabilities

It never ceases to amaze me how topical these - um - topics - are.  I just
sent a box of boards out last nught to an x-ray shop.  (same boards I asked
about earlier, this time with lead free BGAs).  We're getting strange results and
assumed there's opens in the BGA.  I don't have a lot of confidence that the
used a hot enough profile for a big board with many copper planes, so I'm
expecting some non-wetting.

Can I assume from this thread that they very well might give these boards a
passing grade, yet we could still have opens?  The lab says they can do angle
x-rays, we turned down another shop that said they do top-down only.

One of the suspected opens is in row 2.  What about a BGA scope for that
one?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2