Oh I see what you mean it's probably easier to find HOP than a coplanar
defact at the board leel.
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Willis
Sent: Wednesday, October 07, 2009 11:05 AM
To: [log in to unmask]
Subject: Re: [TN] BGA X-Ray Defect Detection Capabilities
To have a heat in pillow you need solder on the pad and the open between the
dish of the solder and the ball surface hence the contamination on the
surface of the ball?
Have a GREAT Day from downtown San Diego
Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
www.ASKbobwillis.com
www.SolderingStandards.com
New Package on Package Workshops 24th November
www.ASKbobwillis.com/PoPWorkshops.pdf
PCB Design for Manufacture & Assembly Workshop 15th October
www.ASKbobwillis.com PCB Inspection & Quality Control Workshop 3rd November
www.ASKbobwillis.com/faworkshops.pdf
Book Bob's "Step by Step Failure Analysis Workshop" 4th November
www.ASKbobwillis.com/faworkshops.pdf
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: 07 October 2009 18:21
To: [log in to unmask]
Subject: Re: [TN] BGA X-Ray Defect Detection Capabilities
No apology needed Bob, sounds like an argument of whether you put water in
the whiskey or whiskey in the water, either way to a purist it is a bad
thing.....8-)
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Willis
Sent: Wednesday, October 07, 2009 6:56 AM
To: [log in to unmask]
Subject: Re: [TN] BGA X-Ray Defect Detection Capabilities
Sorry JB you need to coat a couple of balls to create the defect then place
the device not the pads!!!! O dear I am giving away how I make my video
clips.
Did you like all the sepia tone images of SMART Group's 25th Anniversary in
the newsletter, you giving me a big tube of smarties as a gift for being
Chairman was nice!!!
Many thanks
Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
www.ASKbobwillis.com
www.SolderingStandards.com
New Package on Package Workshops 24th November
www.ASKbobwillis.com/PoPWorkshops.pdf
PCB Design for Manufacture & Assembly Workshop 15th October
www.ASKbobwillis.com PCB Inspection & Quality Control Workshop 3rd November
www.ASKbobwillis.com/faworkshops.pdf
Book Bob's "Step by Step Failure Analysis Workshop" 4th November
www.ASKbobwillis.com/faworkshops.pdf
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: 06 October 2009 18:16
To: [log in to unmask]
Subject: Re: [TN] BGA X-Ray Defect Detection Capabilities
It is very difficult to find co-planar board surface defects on Xray. The
system relies on a visual interpretation for example an elongated joint
profile suggests some level of co planarity issue such as component warpage
- If all joints are good except one or two non wets the X-ray system may
have issues resolving this.
The reason is that the "pull down" of the good joints will compress the
molten solder on the open joint that cannot wet to the pad and it will not
look too much different from the joints around it.
If you want to manufacture such a joint you could deliberately contaminate
one or two BGA pads, reflow the BGA and then go take a look on the Xray
system to see if you can resolve it.
I am not going to tell you how to contaminate those pads (you should not
have an issue) as there are people here that will yell at me.........8-)
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: Tuesday, October 06, 2009 8:56 AM
To: [log in to unmask]
Subject: [TN] BGA X-Ray Defect Detection Capabilities
Everyone,
I just came back from an X-ray vendor qualification trip, and of course,
have a few questions for my professional peers.
Both vendors experienced problems reliably detecting opens and non-wets.
I really didn't expect to see this, as I thought these would be two of the
most common defects seen among BGA users. We had to leave boards at both
facilities so they could further develop their algorithms.
We were not able to create a head-in-pillow defect, and thus, were not able
to check their machines for this. They also had no sample boards that
carried such an anomaly. Is this another defect that is difficult to
detect, and must one utilize a 3D machine in order to find it (assuming the
machine is capable of both 2D and 3D inspections, and there are no
components beneath the BGA)?
Are there any other caveats you might be able to provide? Our list of
questions and qualification efforts were extensive, but I'm certain we
missed something. I just hope whatever it was fell outside of being a
critical item...
Thanks in advance,
Leland
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|