TECHNET Archives

October 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Leland Woodall <[log in to unmask]>
Date:
Tue, 6 Oct 2009 16:09:20 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-Transfer-Encoding:
quoted-printable
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (292 lines)
Hi Leland! We have integrated Xray technology in our BGA processes as a 
very success process control protocol. The primary use of Xray technology 
for us is solder ball/joint uniformity, void analysis and component 
placement/location. Xray technology doesn't find everything but is a good 
tool to have. Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




Leland Woodall <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
10/06/2009 01:18 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Leland Woodall <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] BGA X-Ray Defect Detection Capabilities






Sounds like I?ve been led down a rosy pathway.  I thought these machines 
would do everything but serve you a cup of coffee.

 

Both of them were 3D with an option to inspect in 2D (or provide a 
combination of the two).  If the 3D option is utilized and indeed 
inspecting every solder joint on one BGA, can the machine be ?tweaked? 
enough to assure we?ll catch all the opens, non-wets, and head-in-pillows?

 

If not, I?ve got to back up and punt, and the defensive line is bearing 
down quickly!  Are there any other suggested options (other than not 
building a defect in the first place)?

 

Nothing ever goes as planned?

 

Leland

 

From: [log in to unmask] [mailto:[log in to unmask]] 
Sent: Tuesday, October 06, 2009 1:44 PM
To: [log in to unmask]; Leland Woodall
Subject: Re: [TN] BGA X-Ray Defect Detection Capabilities

 

Hi Leland,
John Burke gave you good advice. Forget 2-D for the defects you are 
interested in, and 3-D is not much better except for some very specialized 
machines that look at SJs individually?bad part is of course, not very 
useful in mass production.
Werner

 

 

-----Original Message-----
From: Leland Woodall <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, Oct 6, 2009 11:55 am
Subject: [TN] BGA X-Ray Defect Detection Capabilities

Everyone,









I just came back from an X-ray vendor qualification trip, and of course,




have a few questions for my professional peers.









Both vendors experienced problems reliably detecting opens and non-wets.




I really didn't expect to see this, as I thought these would be two of




the most common defects seen among BGA users.  We had to leave boards at




both facilities so they could further develop their algorithms.









We were not able to create a head-in-pillow defect, and thus, were not




able to check their machines for this.  They also had no sample boards




that carried such an anomaly.  Is this another defect that is difficult




to detect, and must one utilize a 3D machine in order to fi
nd it




(assuming the machine is capable of both 2D and 3D inspections, and




there are no components beneath the BGA)?









Are there any other caveats you might be able to provide?  Our list of




questions and qualification efforts were extensive, but I'm certain we




missed something.  I just hope whatever it was fell outside of being a




critical item...









Thanks in advance,









Leland









---------------------------------------------------




Technet Mail List provided as a service by IPC using LISTSERV 15.0




To unsubscribe, send a message to [log in to unmask] with following text in




the BODY (NOT the subject field): SIGNOFF Technet




To temporarily halt or (re-start) delivery of Technet send e-mail to 




[log in to unmask]: SET Technet NOMAIL or (MAIL)




To receive ONE mailing per day of all the posts: send e-mail to 




[log in to unmask]: SET Technet Digest




Search the archives of previous posts at: http://listserv.ipc.org/archives




Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for 




additional information, or contact Keach Sasamori at [log in to unmask] or 




847-615-7100 ext.2815




-----------------------------------------------------






---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2