TECHNET Archives

September 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Linda Langley <[log in to unmask]>
Date:
Fri, 18 Sep 2009 12:19:47 +0000
Reply-To:
Subject:
From:
Vladimir Igoshev <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Type:
text/plain
Content-Transfer-Encoding:
base64
Parts/Attachments:
text/plain (1 lines)
Not necessarily. It depends on the board finish.



Vladimir

SENTEC

11 Canadian Road, Unit 7.

Scarborough, ON M1R 5G1

Tel: (416) 899-1882

Fax: (905) 882-8812

www.sentec.ca





-----Original Message-----

From: Linda Langley <[log in to unmask]>



Date:         Fri, 18 Sep 2009 07:54:10 

To: <[log in to unmask]>

Subject: Re: [TN] Black Pad





Werner,

Would the pads and via holes be black if it is brittle interfacial

separation?



Linda Langley CIT

Training Specialist

Jabil Circuit

248-292-6176



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /*

Sent: Friday, September 18, 2009 7:02 AM

To: [log in to unmask]

Subject: Re: [TN] Black Pad





 Hi Linda,

'Black Pad,' by definition is unique to ENIG.

However, there has been some sloppy usage to brittle interfacial

failures in general. Brittle interfacial separations are possible for

almost any surface treatment, but they are not 'black pad' which is a

high concentration of nickel-phosphide at the interface of the

Ni-deposit and the SnNi-IMC, which weakens this interface.

Werner





 





 



-----Original Message-----

From: Linda Langley <[log in to unmask]>

To: [log in to unmask]

Sent: Fri, Sep 18, 2009 6:12 am

Subject: [TN] Black Pad





















I know we have had this subject many times before so I did go to the

archives and still can't find an answer. My question, is Black Pad only

associated with ENIG? Is it possible with immersion Tin?



 



Linda Langley CIT



Training Specialist



Jabil Circuit



248-292-6176





---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to 

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to 

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 

additional information, or contact Keach Sasamori at [log in to unmask] or 

847-615-7100 ext.2815

-----------------------------------------------------







 





---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------




ATOM RSS1 RSS2