Lee
It's better quality than mine,
(not a copy of a copy of a..., you can even see the staple holes from when
it was singulated to go through machine!)
Looks like a handy place for other stuff too, so thanks.
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee Whiteman
Sent: 29 July 2009 14:03
To: [log in to unmask]
Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT
I found the paper, "Effect of Au on the reliability of fine pitch
surface mount solder joints" at this hyperlink:
http://www.osti.gov/bridge/servlets/purl/5208317-1FSVKm/5208317.pdf
We had a serious problem with Gold (Au) with one of our suppliers, hence
my curiosity. Glancing at it, the paper looks pretty interesting.
Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
Sent: Wednesday, July 29, 2009 6:34 AM
To: [log in to unmask]
Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER
JOINT
EPP or at least EPP Europe is still in existence
http://www.epp-online.de/epp/live/start/1.html
However If you Google the words in the title you will find a number of
libraries who will sell you a copy of the paper.
On my HDD I find I have a copy of a paper
"Effect of Au on the reliability of fine pitch surface mount solder
joints"
By Glazer - Hewlett Packard, Kramer - University of California and
Morris -
Lawrence Berkeley Laboratory which is pertinent.
Finally you can down load an Application Note "Soldering to gold" which
deals with this topic at a lower, pragmatic level.
http://www.indium.com/techlibrary/applicationnotes.php
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: 29 July 2009 00:18
To: [log in to unmask]
Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER
JOINT
Jon,
You will have to go to a library, probably a tech one or a big one. I
have
only been able to find sporadic issues from November 2000 to June 2003
on
line.
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gervascio, Thomas L
Sent: Tuesday, July 28, 2009 6:42 PM
To: [log in to unmask]
Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER
JOINT
How could I get a copy of it? I thought EP&P was out of print..
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Tuesday, July 28, 2009 10:01 AM
To: [log in to unmask]
Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER
JOINT
Hi Jon - the folks from Lockheed published a very good article on the
impact
of gold on solder joints including the calculations/material
parameters/graphs that would be useful to you. Pull a copy of this
article: "Effects of Gold Diffusion on a Near Eutectic Solder Joint", S.
Enwright, Electronic Packaging & Production, June 1998, pp 68-72. Good
Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
"Roberts, Jon (SA-1)" <[log in to unmask]> Sent by: TechNet
<[log in to unmask]>
07/28/2009 07:53 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to "Roberts, Jon
(SA-1)" <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT
Does anyone have or know where to find the formula for determining the
amount of percentage of gold in a SMT solder joint? Appreciate any
help, Jon
This communication is intended only for use by the addressee(s) named
herein and may contain business confidential and/or legally privileged
information. If you are not the intended recipient of this e-mail, you
are
hereby notified that any dissemination, distribution, disclosure or
copying of this e-mail and its contents is strictly prohibited. If you
have received this e-mail in error, kindly notify the sender by replying
to this message. In addition, please permanently delete the message and
any attachments without copying or disclosing the contents. Thank you
for
your cooperation.
THIS DOCUMENT AND/OR SHIPMENT MAY CONTAIN COMMODITY ITEMS, SOFTWARE OR
TECHNICAL DATA THAT IS CONTROLLED BY U.S. EXPORT LAW, AND MAY NOT BE
EXPORTED OUTSIDE THE UNITED STATES OR TO NON U.S. PERSONS WITHOUT THE
APPROPRIATE EXPORT LICENSE FROM EITHER THE U.S. DEPARTMENT OF STATE OR
DEPARTMENT OF COMMERCE.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content, and any files transmitted with it, are
intended solely for the addressee(s) and may be legally privileged
and/or confidential. If you are not the intended recipient, please
contact the sender by return and delete the material from any computer.
Any review, retransmission, dissemination, or other use of, or taking of
any action in reliance upon this information by persons or entities
other than the intended recipient is prohibited.
Messages sent via this medium may be subjected to delays, non-delivery,
and unauthorized alteration. This email has been prepared using
information believed by the author to be reliable and accurate, but
Indium Corporation makes no warranty as to accuracy or completeness.
Indium Corporation does not accept responsibility for changes made to
this email after is was sent. Any opinions or recommendations expressed
herein are solely those of the author. They may be subject to change
without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after is was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|