TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 19 May 2009 15:07:46 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Werner Engelmaier /* <[log in to unmask]>
Content-Type:
text/plain; charset="utf-8"
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (253 lines)
 Bev,
You missed the biggest disadvantage—it is destructive.
I would think the completeness of underfill coverage depends at least to some degree on the degree of the quality of the flux removal process underneath the component. Thus, I would think you will find something different with each component. 
Having a destructive method may give you 100% scrap, 8-(
Werner


 


 

-----Original Message-----
From: Bev Christian <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, 19 May 2009 2:54 pm
Subject: Re: [TN] Underfill Pass/fail criteria










Ioan,

Well if you don't have any expletive deleted RF cans in the way, you can use 
acoustic microscopy.  Otherwise your choices are:

1) Prying

2) Vertical cross-sectioning

3) Horizontal cross-sectioning

 

Here blow are my perceived advantages and disadvantages of each. I pasted the 
table in as HTML.  Hope this shows up in TechNet!

 

Method

Advantages

Disadvantages

Prying

Fast, easy, can be done by anyone, checks whole area under component at once

Misses embedded voids that don't reach the underfill/component interface

Vertical Cross-sectioning

Finds buried voids

Requires lab staff, only finds voids in the particular plane sectioned, unless 
grind further (very time consuming)

Horizontal cross-sectioning

Finds buried voids, checks whole area under component

Requires lab staff, very time consuming

 

Bev

RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Tuesday,20May 19, 2009 2:40 PM
To: [log in to unmask]
Subject: Re: [TN] Underfill Pass/fail criteria

 

Bev,

 

No answer here, but one question: how can one visualize and measure voiding in 
underfills?

 

Thanks,

 

Ioan Tempea, ing.

t : 450-967-7100 ext : 244

[log in to unmask]

www.digico.cc

P N'imprimer que si nécessaire - Print only if you must

-----Message d'origine-----

De : Bev Christian [mailto:[log in to unmask]] 

Envoyé : 19 mai 2009 13:52

À : [log in to unmask]

Objet : [TN] Underfill Pass/fail criteria

 

TechNetters,

I am aware of J-STd-030 "Guideline for Selection & Application of

Underfill" and the existence of IPC standards committee 5-24F "Underfill

Adhesives for Flip Chip Applications".  There is nothing in IPC-A-610D

about underfills.  I have taken Brian Toleno's very good course on

underfills, but on going back and looking at the CD, I don't see

anything on pass/fail criteria.  Do any of you know of an international

standard (American, IEC, Japanese) with pass/fail criteria for cured

underfills?

 

I am particularly interested in what said standard (or anything you want

to tell me) says about coverage and voiding.

 

Bev

RIM

 

---------------------------------------------------------------------

This transmission (including any attachments) may contain confidential 
information, privileged material (including material protected by the 
solicitor-client or other applicable privileges), or constitute non-public 
information. Any use of this informa
tion by anyone other than the intended 
recipient is prohibited. If you have received this transmission in error, please 
immediately reply to the sender and delete this information from your system. 
Use, dissemination, distribution, or reproduction of this transmission by 
unintended recipients is not authorized and may be unlawful.

 

---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815

-----------------------------------------------------

 

---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET T
echnet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815

-----------------------------------------------------


---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential 
information, privileged material (including material protected by the 
solicitor-client or other applicable privileges), or constitute non-public 
information. Any use of this information by anyone other than the intended 
recipient is prohibited. If you have received this transmission in error, please 
immediately reply to the sender and delete this information from your system. 
Use, dissemination, distribution, or reproduction of this transmission by 
unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information,=2
0or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2