You need to talk to the Tyco engineer to verify how the connector was qualified and on what tooling. With the fine stranding the Tyco engineer may suggest different crimp dies or connector.
Fred Miller
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Forrester, Michael (H
USA)
Sent: Monday, April 06, 2009 12:05 PM
To: [log in to unmask]
Subject: [TN] Wire Crimps: Machine Vs Hand Tool Specs
We have an application that uses a tyco 350550-2 crimped on connector.
It is being crimped onto
a 14AWG wire made up of 1050 strands of 44 AWG wire. The wire has a
nom. wall of .015" and an
nom OD of .115". The standard pull test calls out for min 50 lbs. If
we crimp it in automated machines
per spec to .069" crimp height, we fail the pull test at an avg of 47
lbs. If we hand crimp it to spec at
.063", we get a pull strength avg of 55 lbs., which passes. Due to the
volume, the automated machine
process is preferred. I have two questions: 1) Why are the automated and
hand tool crimp height
specifications different? 2)Is there an issue with just setting up the
automated tool to the hand tool
crimp height specifications? Thank you.
Best Regards,
Michael Forrester
Sr. Product Engineer
Siemens Healthcare Diagnostics
101 Silvermine Rd.
Brookfield, CT 06804
PH: (203) 740-6452
The attachment named could not be scanned for viruses because it is a password protected file.
----------------------------------------------------------------------------
This message and any included attachments are from Siemens Medical Solutions
and are intended only for the addressee(s).
The information contained herein may include trade secrets or privileged or
otherwise confidential information. Unauthorized review, forwarding, printing,
copying, distributing, or using such information is strictly prohibited and may
be unlawful. If you received this message in error, or have reason to believe
you are not authorized to receive it, please promptly delete this message and
notify the sender by e-mail with a copy to [log in to unmask]
Thank you
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|