well sounds like it's not yet been established whether failure is
component, solder assembly or pwb. Questions about financial
responsibility are mute at this point.
Werner gave good advice/perspective in his comments.
dw
At 12:48 AM 4/7/2009, Karnwal, Pankaj wrote:
>Hi Dwight Mattix
>
>I am agree with you, :-)
>
>But first thing comes in my mind that, have the board is not repaired
>yet to identify the reason of failure ??
>
>We usually do the step analysis :
>1. Simulate the reported problem on our test Jig / end product.
>2. Reason detection of failure with out disturbing the board by
>physically ( Resoldering, tightening of connection ) and electronically
>( Reloading the firmware, upgrading )
>3. Once reason is detected/suspected, like failure of component,
>soldering issue, we do the repair activity, with preservation of data,
>like photo graph of affected area , X-ray images, copy the firmware.
>4. If repair activity is done successful, then confirmation of fault is
>important by the revert back the situation.
>5. One the reason or fault location is confirmed then root cause
>analysis of failure is starts...
>
>If component is defective then it can be send to the component Mfg. to
>FA ( Failure analysis ).
>
>You are seems to be lucky you found a permanent nature of fault, it can
>be easily addressed, in case of intermittent failure it becomes 10 times
>difficult :-)
>
>BR
>Pankaj Karnwal
>Engineer QA
>
>Barco Electronics System Ltd.
>India
>
>Save Environment for future
>
>
>
>
>-----Original Message-----
>From: Dwight Mattix [mailto:[log in to unmask]]
>Sent: Monday, April 06, 2009 7:12 PM
>Subject: Re: PCB Failure analysis
>
>There's always two conversations going on in these matters. Be careful
>not to mix them too soon.
>
>One is technical/scientific. The other is about business/financial
>responsibility. Don't start the second conversation prematurely.
>
>First things first. Answer first question while keeping your technical
>hat firmly in place -- before going on to discuss second matter.
>
>Have you (or the customer) done a failure analysis yet? Have you been
>able to isolate on the failure and categorize the failure mode(s)?
>
>The second matter is more difficult.
>
>Been there. Done that. Got the tee-shirt. Weekly. :-)
>
>Good luck.
>
>At 10:05 PM 4/5/2009, mp3 wrote:
> >Hello,
> >
> >One of our customers have comeback after 3 years asking for a failure
> >analysis report on a 10 layer industrial grade PCB. The PCB was
> >supplied 3 years back and has been functioning satisfactorilly for the
> >last 3 years. Now the customer has 3 PCBs which have failed and is
> >insisting it is a PCB related failure. The failure in all the
> >3 circuit boards are in the same area around a quadpack IC. We verified
>
> >the traveller card of the boards processed and found all aspects to be
> >compliant. The PCBs were being used in a jig for high reliability
> >harness checking. We feel it should be a component related issue rather
>
> >than a PCB related issue.
> >
> >Can you give us some inputs on the above which will help us in arriving
>
> >at the right conclusion.
> >
> >Rgds
> >
> >Pradeep
> >
> >-------------------------------
> >Micropack Ltd, Bangalore, India
> >
> >---------------------------------------------------
> >Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> >unsubscribe, send a message to [log in to unmask] with following text in
> >the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> >or (re-start) delivery of Technet send e-mail to
> >[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
> >per day of all the posts: send e-mail to
> >[log in to unmask]: SET Technet Digest
> >Search the archives of previous posts at:
> >http://listserv.ipc.org/archives Please visit IPC web site
> >http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> >information, or contact Keach Sasamori at [log in to unmask] or
> >847-615-7100 ext.2815
> >-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
>unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
>(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
>archives of previous posts at: http://listserv.ipc.org/archives Please
>visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
>additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>
>DISCLAIMER:
>Unless indicated otherwise, the information contained in this
>message is privileged and confidential, and is intended only for the
>use of the addressee(s) named above and others who have been
>specifically authorized to receive it. If you are not the intended
>recipient, you are hereby notified that any dissemination,
>distribution or copying of this message and/or attachments is
>strictly prohibited. The company accepts no liability for any damage
>caused by any virus transmitted by this email. Furthermore, the
>company does not warrant a proper and complete transmission of this
>information, nor does it accept liability for any delays. If you
>have received this message in error, please contact the sender and
>delete the message. Thank you.
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|