this is little odd question in this forum, but I try:
after machining a complex structure in pure Titanium, how do you clean the
part to a medical cleanliness level?
Threading/cutting oil was a mineral oil with added Sulphur and Zinc /MSDS
7047. I have an idea about alcaline cleaning with
ultrasonic followed by etching in a 10% water/HNO3 solution, ended with
ultrasonic water washing in distilled water.
Anyone with experience?
/Inge
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------