TECHNET Archives

October 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Kane, Amol (349)" <[log in to unmask]>
Date:
Tue, 7 Oct 2008 17:12:36 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Lee Whiteman <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (97 lines)
Amol,

In a prior life (or two), I tried soldering SnBi with hand soldering and
reflow soldering. My impression was that it did not wet well, despite
the lower melting point. At that time, if I had to select a Lead Free
Solder, I would not go with SnBi. 

However, that was several years ago and I have not tried it since then.
Assuming that the solder manufacturers increased the flux activity
since, I would consider it for non aerospace applications where I have
heard that it has been used successfully. Otherwise, I would not use it
for high reliability or aerospace applications, IMHO.

Hope this helps.

Good Luck.

Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]
 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Amol (349)
Sent: Tuesday, October 07, 2008 11:57 AM
To: [log in to unmask]
Subject: [TN] Sn-Bi Alloy for soldering

Does anybody have any experience with Sn-Bi alloy used for soldering
lead-free boards? I am looking at literature available out there and see
Sn-Bi used as a surface finish for components, but I have not yet found
a reference where it is used for soldering.

Looking for pros/cons, good/bad experiences and things to look out for
during soldering.

The application is all SMT, with a temp sensitive part. The manufacturer
therefore wants to use Sn-Bi alloy as this is a lower melting point
alloy

Regards,
Amol





WARNING:  Export Control 
This document may contain technical data within the definition of the 
International Traffic in Arms Regulations (ITAR), and subject to the
Export 
Control Laws of the U.S. Government.  Transfer of such data by any means
to a 
foreign person, whether in the United States or abroad, without proper
export 
authorization or other approval from the U.S. Department of State is 
prohibited. 
 
CONFIDENTIALITY NOTICE: 
This e-mail, and any attachments, is for the sole use of the intended 
recipient(s) and may contain information that is confidential and 
protected from disclosure under the law. Any unauthorized review, use, 
disclosure, or distribution is prohibited. If you are not the intended 
recipient, please contact the sender by reply e-mail, and delete/destroy

all copies of the original message and attachments. 
Thank you.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2