TECHNET Archives

October 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Wed, 15 Oct 2008 15:13:15 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Chris Schaefer <[log in to unmask]>
Subject:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="windows-1252"
From:
Chris Schaefer <[log in to unmask]>
Parts/Attachments:
text/plain (27 lines)
Hey all,

There is a big hubub about how our Static Ionic test machine (600SMD) 
should be configured. Meaning what industry standard and its interpretation 
dictates if the machine should be setup in auto-terminate mode or set a timed 
mode. Is a heating solution better for enabling improved measurement of OA 
species or rosin species. We use our machine to measure product coming off 
of two cleaning processes - one hot DI water and other semi-aqueous using 
soap hot DI water. I interpret the standard as saying that the test should 
continue until there is no more change in conductivity - thus meaning that it 
should be in auto-terminate mode letting the machine do the math and shut 
down when no change is measured.

Any thoughts... Thanks in advance.

Chris

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2