TECHNET Archives

October 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Thu, 30 Oct 2008 15:30:20 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Pete Houwen <[log in to unmask]>
Subject:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="windows-1252"
From:
Pete Houwen <[log in to unmask]>
Parts/Attachments:
text/plain (24 lines)
I have a sudden appreciation for this thread, as I just received a lab report on 
my mystery gold plated boards from a month or so back.

These were the ENiG boards with a flat but scratched looking surface.  
Randomly located XRF measuremenents show Au thicknesses anywhere from 
2.2ui to 8.2ui.  Rough estimating, the gold thickness=solder paste thickness, I 
wonder what percentage of gold I'll find in those joints?

But at least they finally explained why they sent such a terrible microsection 
with their sample boards.  They accidently sent the one they meant to 
reject.  As though it's a cure for my insomnia or something........

Peter

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2