Thanks for the email, Dave. I sure wish I had had the chance to chat
with you when you were here for the SMTA meeting awhile back.
Regarding the mixed alloy scenario, I just wanted to make sure that if
"leaded" assemblies are held at higher reflow temps for longer times in
order to accomplish a more thorough mix in the Pb-free BGA ball alloy,
that people understand there may be other (expensive) parts that cannot
withstand this, and the component vendors will take themselves off the
hook from a warranty standpoint if their components are subjected to
higher-than-recommended temperatures.
Another thought I forgot to mention is that the rest of the leaded
assembly can be spared the higher reflow temperature of the "rogue"
Pb-free BGA if the Pb-free BGA is soldered to its own little interposer
substrate with Pb-free solder paste and a Pb-free profile, and then this
subassembly is subsequently soldered to the assembly using 63/37 paste
and standard reflow profile. The interposer bottom-side solder balls can
be 63/37, and of course they will go into liquidus during reflow of the
subassembly, but that does no harm if flux is applied.
Companies like Gryphics www.gryphics.com and Analog Technologies
www.analog-tech.com make COTS array-to-array interposers and
subassemblies just for this application, for almost any component on the
market.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Tuesday, October 21, 2008 2:38 PM
To: [log in to unmask]
Subject: Re: [TN] Lead Free BGA'S
Hi Richard - your comments provide good additional ideas to keep in
mind.
The folks at Celestica (Dr. Polina Snugovsky and crew) have published a
couple of papers since my paper first was released to the public which
are very good and give a better overall bandwidth discussion on the
different aspects of achieving good solder joint integrity in a mixed
situation. One issue I know that all of the "camps" include in their
discussions is the impact of the increased reflow temperature on the
integrity of the tin/lead solder process qualified components. Your
"Camp C" option is a good attempt to find a solution and balance all of
the competing advantages/disadvantages. Richard Coyle published a good
paper at the 2008 SMTAI Conference with contained some excellent data on
the impact of mixing. I am hoping that we get a few more papers this
year from the industry research that show the impact of a hybrid
situation in a product type test.
Dave
"Stadem, Richard D." <[log in to unmask]> Sent by: TechNet
<[log in to unmask]>
10/21/2008 12:03 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to "Stadem,
Richard D." <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Lead Free BGA'S
I echo Dave Hillman's response, with some additional considerations. I
am of Camp C, which sort of agrees with Camp A and also Camp B. But Camp
C is very concerned with trying to reflow lead-free BGAs using a 63/37
paste and profile, albeit slightly higher, which I think is the "hybrid"
reflow profile which John's assembly house is probably using. The
concern here is that the circuit board material and the components
themselves were probably not selected and/or qualified to be subjected
to the higher reflow temperatures and longer times needed to achieve the
completely mixed (homogenous) alloy. In addition, I know of no studies
or industry data that tested this particular alloy combination.
I would have to say that if you are attempting to reflow this
combination, and are also using ENIG as a surface finish, the risks of
running into issues with the solder joint reliability, the via
reliability, and the rest of the component's reliability are stacked
against you.
I cannot say enough good things about Dave's paper on the subject. I
used it as a reference document in my paper published in this month's
Circuits Assembly magazine. I think if you read both papers you will
come away with a better understanding of the risks of assembling the
Pb-free BGAs using leaded solder. What will become very clear to you is
that you should never attempt to do this without fully qualifying the
process to ensure you are not doing something harmful to the rest of the
components and/or the circuit board itself, so you do not end up with a
huge problem later. As you can see by some of the other respondents,
that is what happened to them, and they are certainly not the only ones
that this happened to. I have been called in to look at this issue more
than once, and it gets real expensive in a hurry.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Tuesday, October 21, 2008 11:23 AM
To: [log in to unmask]
Subject: Re: [TN] Lead Free BGA'S
Hi John! Well, I have a response that probably isn't what you are
looking for - " it depends" (cha-ching, Doug gets another Mt. Dew).
There are two basic camps out in the industry: Camp A: don't use a
lead-free BGA in a tin/lead solder process because you just don't know
what the resulting solder joint may be; (2) Camp B: increase the reflow
temperature so that the lead-free BGA in a tin/lead solder process can
reach a uniform distribution of Pb throughout the solder joint. Some of
the published reports also indicate that the BGA construction specifics
(i.e. material type, die size, I/O, ball metallurgy, e.g.) can play a
significant role in whether the solder joint integrity would be
compromised. The
2006/2007/2008 SMTAI Conference proceedings are good sources of
published papers on the topic. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
John Foster <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
10/21/2008 10:21 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
[TN] Lead Free BGA'S
Our assembly house recently assembled some boards with Lead Free BGA's
for
us
and when I asked them if they used a lead free process they responded
with.
We use leaded solder (Sn63Pb37) with a hybrid oven profile to
accommodate
the lead-free BGA. I hope this answers your question. Please let me know
if you have any more questions."
Is this a common process, is this a reliable process
Any input is appreciated
Thank You
John Foster
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|