Hi John! Well, I have a response that probably isn't what you are looking
for - " it depends" (cha-ching, Doug gets another Mt. Dew). There are two
basic camps out in the industry: Camp A: don't use a lead-free BGA in a
tin/lead solder process because you just don't know what the resulting
solder joint may be; (2) Camp B: increase the reflow temperature so that
the lead-free BGA in a tin/lead solder process can reach a uniform
distribution of Pb throughout the solder joint. Some of the published
reports also indicate that the BGA construction specifics (i.e. material
type, die size, I/O, ball metallurgy, e.g.) can play a significant role in
whether the solder joint integrity would be compromised. The
2006/2007/2008 SMTAI Conference proceedings are good sources of published
papers on the topic. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
John Foster <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
10/21/2008 10:21 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
[TN] Lead Free BGA'S
Our assembly house recently assembled some boards with Lead Free BGA's for
us
and when I asked them if they used a lead free process they responded
with.
We use leaded solder (Sn63Pb37) with a hybrid oven profile to accommodate
the lead-free BGA. I hope this answers your question. Please let me know
if you have any more questions."
Is this a common process, is this a reliable process
Any input is appreciated
Thank You
John Foster
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|