I did not mean to imply that we solder more than a million joints a
month with VPS, but altogether. I agree with Brian that VPS is not a
good high-volume option. It does work well for the smaller quantities of
backplanes and thicker boards with large or massive component
terminations such as inductors, SMA connectors, etc. It also works very
well for metal-clad boards or thick boards with 2 oz copper ground and
power planes, etc.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: Thursday, October 16, 2008 8:28 AM
To: [log in to unmask]
Subject: Re: [TN] Vapor Phase Soldering - The way Forward?
This would have been better as a continuation of the original thread in
the LF forum.
I can't see it being used for high volume work if only because of the
cost.
Brian
Eric CHRISTISON wrote:
> Subject
> Re: [TN] FW: [LF] Vapor Phase Soldering
>
>
>
>
>
>
> " I should also opine that when soldering RoHS-compliant assemblies
> using lead-free solder paste, you will probably get a much better
> yield with VPS than you ever will with convection. Especially in the
> case of SAC solders. "
>
>
> Richard's statement prompts me to ask a related question.
>
> The subject of vapour phase soldering came up in a review that I
> attended this morning on the qualification of a new semiconductor
> package. It was stated that VP soldering would become a lot more
> popular in the future because of a number of advantages it has over
> hot air when using it on lead free components.
>
> What is the opinion of Technet on this? I'm particularily interested
> on predictions of it's usage for the manufacture of high volume PWB
> assys for consumer electronics.
>
> Thanks,
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|