TECHNET Archives

October 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 13 Oct 2008 09:49:37 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Eric CHRISTISON <[log in to unmask]>
Subject:
From:
Eric CHRISTISON <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-1; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (41 lines)
Interesting post Mike,

At the risk of going a little off topic I've never quite understood the 
distinction between a solder and a braze. Is there a clear cut 
difference in the metallurgy of the different joints?

Regards,




> The usual wisdom on soft solders is that they aren't very strong, so the
> more ductile the alloy the less likely it is to break. This conventional
> wisdom doesn't really apply to Au/Sn as it is more like a braze with tensile
> and sheer about 8x 10x lead alloys.
>   

-- 
Eric Christison Msc
Mechanical Engineer
Consumer & Micro group
Imaging Division

STMicroelectronics (R&D) Ltd
33 Pinkhill
Edinburgh EH12 7BF
United Kingdom

Tel:	+44 (0)131 336 6165
Fax:	+ 44 (0)131 336 6001

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2