Hi Tushar,
Look at the units: mils vs. mm.
This is what I believed:
IPC-The stress will be on component body as the joint form is with
"lots" of solder volume.
Supplier - The stress will be on solder joints as it is the weakest
compared to the component body.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mankeekar Tushar
Sent: Friday, 10 October 2008 12:54 PM
To: [log in to unmask]
Subject: [TN] Technical query: Land Patterns SMD
Hi,
I am using the IPC 7351 LP Viewer Version 7.03.00 to ascertain the
Solder Land Patterns of Chip Type Resistors in my PCB design.
I have the following query -
The Viewer shows the following dimensions for Vishay and Panasonic
respectively.
Vishay RESC0603X28N: Pad X= 0.40, Pad Y= 0.45, Pad Space C= 0.70
Panasonic RESC0603X30N: Pad X= 0.40, Pad Y= 0.45, Pad Space C= 0.70
However based on the component datasheets specs I work out the following
dimensions.
Vishay 0603: Pad X= 0.50, Pad Y= 0.9, Pad Space C= 1.5
Panasonic 0603: Pad X= 0.65, Pad Y= 0.9, Pad Space C= 1.45
Can someone please help me clarify my query?
Regards,
--Tushar
Adjudged one of India's top "25 Best Places to work - 2008" by Economic
Times and the Great Places to Work Institute
******************************************
" Call 92256 37451 - Your helpline for everything in Steam "
DISCLAIMER:This e-mail message is proprietary to Forbes Marshall and is
intended solely for the use of the entity to whom it is addressed. It
may
contain privileged or confidential information exempt from disclosure as
per applicable law. If you are not the intended recipient or
responsible for delivery to the intended recipient,you may not
copy,deliver, distribute or print this message. If the contents are
unrelated to
the Company's normal business activity it may be treated as personal
views of the sender. The message and its contents have been virus
checked.
but the recipients may conduct their own. FM will not accept any claims
for damages arising out of viruses.
*******************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|