TECHNET Archives

May 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Tue, 27 May 2008 06:34:44 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, legg <[log in to unmask]>
Subject:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="ISO-8859-1"
From:
Parts/Attachments:
text/plain (28 lines)
I'm curious about the 'leaded' qualification.

Would this be considered the normal, weakest or most likely solder joint to
require rework operations in this consideration?

If so, it doesn't follow my own experience 

- rework to leaded parts being the least stressfull as the part body itself
can often be removed prior to sesoldering the remaining leads and involves
less solder mass per junction 

- rework requirements seem to be random or at least lead-type non-specific 

- some board batches are less rugged to rework than others, regardless of
the board design and process control steps used in their rework. 

RL

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2