TECHNET Archives

May 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 23 May 2008 10:40:33 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Joe Macko <[log in to unmask]>
Parts/Attachments:
text/plain (36 lines)
Techs,

 

I am looking for some help / guidance on how to analytically determine
the number of times the same leaded component can be replaced on a ENIG
finished board before the solder lands located on the PCB have been
degraded beyond their capability to provide a solderable class 3 surface
(.e., how many times can the ENIG finished solder lands with stand a
rework/component remove & replace).  I suspect the dissolution rates of
nickel and copper come into play however I am not sure how to approach
this issue and suspect there are some relatively straightforward
formulas out there to accomplish this task. Everyone has a different
idea and there are numerous rules of thumb discussed but I would like to
try something more analytical (without having to use a supercomputer).
Thanks again and everyone enjoy the long weekend.

 

Best Regards,

-joe

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2