Dan,
First stop would be to contact the manufacturer of the no-clean flux /
solders you use and find out what they recommend. Might not be your final
solution (pun intended), but at least they have some insight into the
composition of the materials and, based on that, can offer up what they
think is the best material to do what you need. They might even have some
suggested methods/materials on their website. I have seen some sites that do
say "If you have to, use..." Usually it's a product that they make (duh!),
but that doesn't mean you have to use it.
Generally speaking I have not seen good results in trying to clean off
no-clean flux. They call it "no-clean" for a reason.
Good luck,
Dale Ritzen
Quality Manager
Austin Manufacturing Services
-----Original Message-----
From: Dan Mauro [mailto:[log in to unmask]]
Sent: Wednesday, March 05, 2008 6:35 AM
To: [log in to unmask]
Subject: [TN] Cleaning No-clean
Folks,
I have a need to clean No-clean residue from PCBA's. Can this be achieved
with water washer and some type of saponifier ? Can anybody suggest a batch
process?
Thanks,
Dan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|