Ioan,
We happen to use March equipment. The March AP 1000 is a batch type system for general purpose use, having multiple gas capability.
You may try http://www.marchplasma.com/ap1000.htm for info on the March line of plasma equipment.
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Thursday, March 20, 2008 1:41 PM
To: [log in to unmask]
Subject: Re: [TN] Shelf life of bare copper boards
Any brands/models I should check?
Thanks,
Ioan
-----Message d'origine-----
De : Hfjord [mailto:[log in to unmask]]
Envoyé : 20 mars 2008 11:48
Ā : 'TechNet E-Mail Forum'; Ioan Tempea
Objet : SV: [TN] Shelf life of bare copper boards
Buy one! You will always have use of it. We couldn't be without it for one
day. Kinda first aid, if you want.
/Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Ioan Tempea
Skickat: den 20 mars 2008 16:25
Till: [log in to unmask]
Ämne: Re: [TN] Shelf life of bare copper boards
The components soldered on the first side are on when populating the second
side.
And no plasma available.
Thanks again,
Ioan
-----Message d'origine-----
De : Hfjord [mailto:[log in to unmask]]
Envoyé : 20 mars 2008 11:20
Ā : 'TechNet E-Mail Forum'; Ioan Tempea
Objet : SV: [TN] Shelf life of bare copper boards
Are there components on already? Then, what do you assemble?
Another trick could be to plasma clean the boards, if you got such a
machine. If the copper oxide isn't too thick Argon bombardment may work.
If you got organic contaminations on top of copper oxide, then I don't know
what to do, depending on what components you have already on the board. If
the components are not sensitive to solvents, you can clean (to remove many
organics) with ordinary cleaning methods, followed by plasma cleaning for
the oxide.
/Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Ioan Tempea
Skickat: den 20 mars 2008 13:09
Till: [log in to unmask]
Ämne: Re: [TN] Shelf life of bare copper boards
Thanks TN for your answers!
My questions come from our ups and downs in assembling a few double sided
FR-4 boards, with exposed copper layers. We see variable batch to batch
soldering quality and believe it is the variable degree of surface oxidation
that is causing the problem.
This product is medium to high volume, so acid dipping or any other
conditioning of the surface would have a large impact on the assembly costs
and eventually on delivery dates.
Of course the double side reflow does not really help and I would hesitate
doing acid dipping when there are components and solder joints on the boards
already.
So what would help me even more would be a few ideas on the packaging we
should request and the handling of the boards. Mike named a few, are there
more suggestions out there?
Best regards and Happy Easter,
Ioan
-----Message d'origine-----
De : Hfjord [mailto:[log in to unmask]]
Envoyé : 19 mars 2008 14:06
Ā : 'TechNet E-Mail Forum'; Ioan Tempea
Objet : SV: [TN] Shelf lif of bare copper boards
Have no idea what strange things you are doing, but an easy way to activate
the copper is to dip the boards in a weak acid solution, strength depending
on the time the boards have been exposed to the atmosphere. Rinse rigorously
in DI !
/Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Ioan Tempea
Skickat: den 19 mars 2008 13:42
Till: [log in to unmask]
Ämne: [TN] Shelf lif of bare copper boards
Dear Technos,
Anybody using PCbs with bare copper pads and traces, no plating, no OSP,
not even solder mask? Because I have a few questions:
What is their shelf life?
Are they suited for double side SMT reflow? I mean, during the first
reflow the oxidizing is accelerated...
What storing/handling procedures you use?
Does the copper require any particular specifications, in order to
perform better in soldering?
Anything else?
Thank you,
Ioan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer. [gntx v.1]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|