TECHNET Archives

December 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Gervascio, Thomas" <[log in to unmask]>
Date:
Thu, 20 Dec 2007 14:59:23 -0500
Reply-To:
Content-Transfer-Encoding:
7bit
Subject:
From:
Guy Ramsey <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Organization:
R&D Assembly
MIME-Version:
1.0
Parts/Attachments:
text/plain (49 lines)
We don't use rubber. We found some glass fiber brushes in a pen-like handle.
They work great. They cut the metal off and do not imbed crap in the copper.
TechniTool? I think that is where we got them. Board repair stuff. 

If you have your heart set on the erasers try a drafting or graphic design
supply store.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gervascio, Thomas
Sent: Thursday, December 20, 2007 2:04 PM
To: [log in to unmask]
Subject: [TN] Erase to abrade off HASL off circuit cards

We have a requirement to use an erase to remove solder from a PCB pad down
to the base copper. The recommended erase is too soft- we found a hard grey
abrasive erase that goes in an electric eraser but don't know where we can
buy more of these. Any ideas?
 
Tom Gervascio
Principal Process Engineer
Sypris Electronics
Desk/VoiceMail    813-972-6763
Beeper                 813-887-0098
 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2