Hi Bob
We specify that the solder mask material must be per a list of materials
we've found work OK. It can be an issue for us - I'd say "it depends"
on how forgiving your coating material is.
regards
- Graham Collins
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wilson, Bob
Sent: Wednesday, November 28, 2007 2:43 PM
To: [log in to unmask]
Subject: [TN] Conformal coating question part 2
Hi,
I found out I'm calling out a somewhat generic note for my soldermask:
"...APPLY GREEN LIQUID PHOTO IMAGEABLE SOLDER MASK PER IPC-SM-840, CLASS
H..."
Then we are spraying the boards using Tech Spray Fine-L-Kote, 2102,
Silicone Conformal Coating.
Is there a better way to specify my board soldermask that will not cause
compatibility issues with this type of conformal coating?
Or is my concern a non-issue?
Thanks a bunch.
Regards,
Bob Wilson
E/M Designer, CID+
SpectraSensors, Inc.
11027 Arrow Route
Rancho Cucamonga, CA 91730
(909) 948-4110
www.spectrasensors.com
www.ipc.org
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|