TECHNET Archives

November 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wilson, Bob" <[log in to unmask]>
Date:
Wed, 28 Nov 2007 14:52:46 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Graham Collins <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (68 lines)
Hi Bob
We specify that the solder mask material must be per a list of materials
we've found work OK.  It can be an issue for us - I'd say "it depends"
on how forgiving your coating material is.  

regards
 - Graham Collins 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wilson, Bob
Sent: Wednesday, November 28, 2007 2:43 PM
To: [log in to unmask]
Subject: [TN] Conformal coating question part 2

Hi,

I found out I'm calling out a somewhat generic note for my soldermask:

"...APPLY GREEN LIQUID PHOTO IMAGEABLE SOLDER MASK PER IPC-SM-840, CLASS
H..."

Then we are spraying the boards using Tech Spray Fine-L-Kote, 2102,
Silicone Conformal Coating.

Is there a better way to specify my board soldermask that will not cause
compatibility issues with this type of conformal coating?

Or is my concern a non-issue?

Thanks a bunch.

Regards,

Bob Wilson
E/M Designer, CID+
SpectraSensors, Inc.
11027 Arrow Route
Rancho Cucamonga, CA 91730
(909) 948-4110
www.spectrasensors.com
www.ipc.org
 
  


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2