TECHNET Archives

April 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Date:
Mon, 30 Apr 2007 15:18:14 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Roland Jaquet <[log in to unmask]>
Subject:
From:
Roland Jaquet <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (111 lines)
Yes Brian, still the same, more choice with 5, 9, 12, ... microns of copper
foils with thicker aluminum backing.

In regards of the Semi-Additive, your basic understanding is correct, but
within the reality, it is more complex.  i.e. surface roughness, dielectric,
etc.. RCC,..  

Meilleures Salutations
Very Best Regards
Roland
 
www.PCBspecialist.com 
Roland Jaquet
14 Champ Budin
1258 Perly, GENEVA
SWTZERLAND
TEL+41-22-880-0405 GSM+41-79-203-3723 FAX +41-22-880-0409
There are three constant in life... Change, Choice & Principles.
Stephen R. Covey

-----Message d'origine-----
De : TechNet [mailto:[log in to unmask]] De la part de Brian Ellis
Envoyé : lundi, 30. avril 2007 10:23
À : [log in to unmask]
Objet : Re: [TN] Question on "semi additive" process

A generation or so ago (I stopped making PCBS in 1974!!!!!), we used to 
buy 5 µm cladded laminate. However, the 5 µm copper was plated onto an 
aluminium substrate before pressing and the laminate was delivered with 
the aluminium (as a guess, probably ~20 µm thick) to protect the fragile 
copper during the mechanical operations. Immediately before laminating 
the resist, we peeled off the aluminium, which we sold as scrap.

The barrel of the PTHS were only about 2-3 µm less than the tracks, 
because the etching fluid was replaced more slowly than the surface in 
the holes because of the capillary effect. We used a copper chloride 
etchant.

I don't know whether 5 µm (or 3 µm) laminate is offered today.

Brian

Adam Seychell wrote:
> I am trying to get a basic understanding on the "semi additive" process. 
> From what I understand, the copper base foil begins at 5um, and circuit 
> traces are electroplated to a desired thickness. Unlike conventional 
> "pattern plating" , there is no metal etch resist, but instead the 
> entire panel is etched just enough to remove the 5um copper base copper, 
> leaving the relatively thicker traces still in tack.
> My question is, what steps are involved in obtaining the 5um copper base
?
> 
> The thinnest copper cladding I can find is 18um (1/2oz) which suggests 
> to me people are deposited 5um of electroless copper on blank PCB 
> insulating material.
> 
> If this is the case then will any of the direct metalization systems be 
> usable ? Due to the plating propagation effect with direct metalization, 
> there would be excessive variations in copper thickness over the whole 
> panel.
> The only alternative I can see is to take standard 18um copper clad and 
> carefully etch down to 5um. The resulting 5um copper clad laminate could 
> then be used with direct metalization systems, however hole walls will 
> not have a 5um base, and therefore the hole wall plating finishes up 
> being 5um thinner than traces.
> 
> 
> regards,
> 
> Adam Seychell
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site 
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 
> ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2