Hi Ed,
TOKO's Change Notice states that the plating is Sn-2Cu, see attachments.
I am trying to find some info on the reflow characteristics of this
alloy as well as compatibility with SnPb solder paste.
Best Regards,
- Joe
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of
[log in to unmask]
Sent: Monday, April 02, 2007 9:34 AM
To: [log in to unmask]
Subject: Re: [TN] Sn-2Cu plating solderability question
Joe, what allow on leads are we talking about? Is it 99.3Sn/0.7Cu? Why
this lead-free alloy and not say SAC305?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Monday, April 02, 2007 12:01 PM
To: [log in to unmask]
Subject: [TN] Sn-2Cu plating solderability question
Good Morning All.
Our inductor supplier, TOKO informed us via PCN that they switched to a
Pb-free, termination plating consisting of Sn-2Cu, which I am not
familiar with. I am looking for some info on this alloy's reflow
requirements as well as compatibility with SnPb solder paste, which is
what we use.
Thanks again
-Joe
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|