Hi Ed, TOKO's Change Notice states that the plating is Sn-2Cu, see attachments. I am trying to find some info on the reflow characteristics of this alloy as well as compatibility with SnPb solder paste. Best Regards, - Joe -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask] Sent: Monday, April 02, 2007 9:34 AM To: [log in to unmask] Subject: Re: [TN] Sn-2Cu plating solderability question Joe, what allow on leads are we talking about? Is it 99.3Sn/0.7Cu? Why this lead-free alloy and not say SAC305? -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask] Sent: Monday, April 02, 2007 12:01 PM To: [log in to unmask] Subject: [TN] Sn-2Cu plating solderability question Good Morning All. Our inductor supplier, TOKO informed us via PCN that they switched to a Pb-free, termination plating consisting of Sn-2Cu, which I am not familiar with. I am looking for some info on this alloy's reflow requirements as well as compatibility with SnPb solder paste, which is what we use. Thanks again -Joe --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------