Allow me to correct my previous statement. SN62 is considered to be an
"alternate alloy" per J-STD-001CS, which is the Space Applications
standard. Within that document, it states that only Sn60Pb40 or Sn63A
are allowed without qualification. Any other alloy (such as Sn96 and
Sn62) shall only be used where specifically indicated by approved
documentation. In addition, any other alloy must meet completely meet
J-STD-006 and be fully qualified and the data presented for approval
before it can be used for space.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Zilber Gil
Sent: Sunday, January 21, 2007 5:02 AM
To: [log in to unmask]
Subject: [TN] Sn63 or Sn62
Hello,
Which solder past is prefer Sn63 or Sn62 for Avionic and military
equipment and for space application (assuming that there are no Ag
components finish?
What are the advantage and disadvantage of each solder past?
Thanks,
Dr. Gil Zilber
Elta system Ltd.
The information contained in this communication is proprietary to
Israel Aerospace Industries Ltd.
and/or third parties, may contain confidential or privileged
information, and is intended only for the use of the intended addressee
thereof. If you are not the intended addressee, please be aware that any
use, disclosure, distribution and/or copying of this communication is
strictly prohibited.
If you receive this communication in error, please notify the sender
immediately and delete it from your computer. Thank you.
This message is processed by the PrivaWall Email Security Server.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|