Allow me to correct my previous statement. SN62 is considered to be an "alternate alloy" per J-STD-001CS, which is the Space Applications standard. Within that document, it states that only Sn60Pb40 or Sn63A are allowed without qualification. Any other alloy (such as Sn96 and Sn62) shall only be used where specifically indicated by approved documentation. In addition, any other alloy must meet completely meet J-STD-006 and be fully qualified and the data presented for approval before it can be used for space. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Zilber Gil Sent: Sunday, January 21, 2007 5:02 AM To: [log in to unmask] Subject: [TN] Sn63 or Sn62 Hello, Which solder past is prefer Sn63 or Sn62 for Avionic and military equipment and for space application (assuming that there are no Ag components finish? What are the advantage and disadvantage of each solder past? Thanks, Dr. Gil Zilber Elta system Ltd. The information contained in this communication is proprietary to Israel Aerospace Industries Ltd. and/or third parties, may contain confidential or privileged information, and is intended only for the use of the intended addressee thereof. If you are not the intended addressee, please be aware that any use, disclosure, distribution and/or copying of this communication is strictly prohibited. If you receive this communication in error, please notify the sender immediately and delete it from your computer. Thank you. This message is processed by the PrivaWall Email Security Server. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------