Hi Kerry - Dr. Hwang's book titled "Environment Friendly Electronics:
Lead-free Technology", ISBN 0-901150-40-1, Chapter 6.2, contains a
significant amount of data on the 58Bi/42Sn solder alloy which may be
helpful in your efforts. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Kerry McMullen
<Kerry_McMullen@L
TX.COM> To
Sent by: TechNet [log in to unmask]
<[log in to unmask]> cc
Subject
12/11/2006 09:01 [TN] 58Bi/42Sn
AM
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
Kerry_McMullen@LT
X.COM
Hello esteemed Technet,
I am looking comments on what you would consider the advantages and
disadvantages of this composition of this solder paste. (58Bi/42Sn)
Lower MP. 138 Degrees C.
Lower fatigue resistance
Wetting to ImAg??
Wetting to ImNiAu??
No Clean? Residue?
Intermetallic Formation?
Mixing with 63/37Sn?
Our application is an RF board where we would use this paste post Wave /
Hand Solder.
Any comments appreciated.
Cheers,
Kerry
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|