TECHNET Archives

December 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 11 Dec 2006 17:33:50 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (78 lines)
Hi Kerry - Dr.  Hwang's book titled "Environment Friendly Electronics:
Lead-free Technology", ISBN 0-901150-40-1, Chapter 6.2, contains a
significant amount of data on the 58Bi/42Sn solder alloy which may be
helpful in your efforts. Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




             Kerry McMullen
             <Kerry_McMullen@L
             TX.COM>                                                    To
             Sent by: TechNet          [log in to unmask]
             <[log in to unmask]>                                          cc

                                                                   Subject
             12/11/2006 09:01          [TN] 58Bi/42Sn
             AM


             Please respond to
              TechNet E-Mail
                   Forum
             <[log in to unmask]>
             ; Please respond
                    to
             Kerry_McMullen@LT
                   X.COM






Hello esteemed Technet,
      I am looking comments on what you would consider the advantages and
disadvantages of this composition of this solder paste. (58Bi/42Sn)
Lower MP.  138 Degrees C.
Lower fatigue resistance
Wetting to ImAg??
Wetting to ImNiAu??
No Clean?  Residue?
Intermetallic Formation?
Mixing with 63/37Sn?
Our application is an RF board where we would use this paste post Wave /
Hand Solder.
Any comments appreciated.

Cheers,
Kerry

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2