Steve,
It's because his co-workers have to work Saturday.
Bill Kasprzak
Moog Inc
Process Engineer, Electronic Assembly
Steve Gregory <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
11/10/2006 08:00 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Steve Gregory <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] NTC - George's Friday Clip...
YAY! It's Friday!
As such, if you remember, George Wenger sent me a clip of how he comes
to work on Monday, and how he goes home on Friday:
http://stevezeva.homestead.com/files/going_Home_Friday.wmv
What I don't understand, is why all of the other co-workers aren't as
happy as George is?
-Steve Gregory-
-----Original Message-----
From: Steve Gregory
Sent: Monday, November 06, 2006 9:46 AM
To: 'Wenger, George M.'; TechNet E-Mail Forum
Subject: RE: [TN] Gold Embrittlement
Yep George, you and me both...hehehe
http://stevezeva.homestead.com/files/going_to_work_monday.wmv
-Steve Gregory-
-----Original Message-----
From: Wenger, George M. [mailto:[log in to unmask]]
Sent: Monday, November 06, 2006 7:53 AM
To: TechNet E-Mail Forum; Steve Gregory
Subject: RE: [TN] Gold Embrittlement
Ingemar,
I needed something to put a smile on my face on a Monday. I typically
have problems on Monday. I've attached an image of how I come to work
on Monday's and have copies Steve for posting.
I just can't wait until Friday comes (second attachment)
Regards,
George
George M. Wenger
Senior Principle FMA / Reliability Engineer Wireless network Solutions
Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 (908) 546-4531
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, November 06, 2006 8:35 AM
To: [log in to unmask]
Subject: Re: [TN] Gold Embrittlement
Mornin' Inge!
Holy Mackerel!! That really shows some embrittlement:
http://stevezeva.homestead.com/files/au_embrittlement.doc
That last picture looks like the bottom of a forest floor! I had a very
small transistor like that one time, and I think I asked the group if I
should tin it. The reason I asked was because it was so small, and I
didn't know if I would damage it by dipping it:
http://www.stevezeva.homestead.com/files/BipolarTransistor.jpg
I'm pretty sure you told me that I had better remove the gold, and now I
know why!
Well, it's the start of another week. I'm really looking forward to
tomorrow being over. I'm so sick of all the political ads I could
scream!
I know this is Monday, but I got sent a picture over the weekend that
will start your week off with a smile. You need to look closely at all
the facial expressions of everybody in the picture:
http://stevezeva.homestead.com/files/Who_Brought_the_Cat.jpg
Have a great week everybody!
-Steve Gregory-
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ingemar Hernefjord
(KC/EMW)
Sent: Monday, November 06, 2006 3:00 AM
To: [log in to unmask]
Subject: Re: [TN] Gold Embrittlement
Agree,
We degold all microwave SMT small outline transistors ("helicopters"),
because we had catastrophic gold embrittlement problems. The solder
joints were so brittle, that the leads lifted from the pad in the temp
cycle tests. We measured as much as 15 micrometers of gold! The
semiconductor manufacturer meant, that it is a problem to have control
on the gold process on such small parts. What nonsense! Anyway, we are
today suspiscious with many gold plated parts and do degolding rather
than getting embrittlement.
I'll send some pictures to Steve, so you can see what can happen.
Horror!
Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: den 2 november 2006 23:06
To: [log in to unmask]
Subject: Re: [TN] Gold Embrittlement
Hi Amol,
I you have imersion Au, Au-embrittlement is not a problem because there
is not enough Au. Be careful, however, if your PCBs come from China; I
have seen much thicker Au-layers than are possible with iAu.
Calculating the wt% of Au in a soldert joint is an exercise in futility,
because you have to make the assumption--frequently not warranted--that
the SnAu-IMCs are uniformally distributed.
In cases where you suspect thicker Au [and for the matter Ag; which is
equally as bad as Au in causing SJ-embrittlement] deposits, the safest
course of action is to wash the Au (Ag) off by tipping.
Werner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
------------------------------------------------------------------------
------------------------
This message is for the designated recipient only and may contain
privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender immediately
and delete the original. Any unauthorized use of this email is
prohibited.
------------------------------------------------------------------------
------------------------
[mf2]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|