TECHNET Archives

November 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 6 Nov 2006 15:00:26 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Subject:
From:
R Sedlak <[log in to unmask]>
Content-Transfer-Encoding:
8bit
In-Reply-To:
Content-Type:
text/plain; charset=iso-8859-1
MIME-Version:
1.0
Parts/Attachments:
text/plain (140 lines)
I agree with Doug Pauls, for all the reasons he specifies, and perhaps some even more important reasons, when it comes to cleaning "no-clean" type fluxes.  "No-cleans" are truly wonderful concepts, the acids form completely insoluble salts with the copper or tin oxides present, and thus are essentially completely inactivated.

Wonderful, unless you need to remove them...

Then you must complex, or chelate, the metals present in the "no-clean" away from chemicals that were chosen to prevent this from occurring.... in order to render the acids soluble... this can only occur in an aqueous system, with some serious chemical power, backed up by a serious energy source (heat and spray).

And, I suppose you need to be assured that it will not attack the board, and/or devices?    You also want it to cure cancer?   That might be easier!

Rudy Sedlak
RD Chemical Company

"Douglas O. Pauls" <[log in to unmask]> wrote: I would agree with Steve.  The Aquanox line has served us well at Rockwell
and we are converting over to the Kyzen Aquanox A4520 and are getting
excellent resuls.  I am a proponent of aqueous cleaning since you get both
the dynamic action of pressurized spray, the thermal activity of hot wash
and rinse waters, and the chemical energy of a saponifier.  For these
reasons, I would strongly recommend you stay away from any kind of vapor
degreasing and no-clean residues.  Bad Karma.

I guess the more important question is why are you cleaning the low solids
flux residues and is the low residue paste designed to be cleanable?  Very
important questions.

Doug Pauls
Rockwell Collins




             Steve Gregory

             TRONICS.COM>                                               To
             Sent by: TechNet          [log in to unmask]
                                                       cc

                                                                   Subject
             11/06/2006 10:05          Re: [TN] Cleaning media for no
             AM                        clean paste


             Please respond to
              TechNet E-Mail
                   Forum

             ; Please respond
                    to
               Steve Gregory

               TRONICS.COM>






Hi Dan!

I've always had very good results cleaning no-clean residues with Kyzen
Aquanox 4512P in a batch cleaner. They have another formula for
lead-free residues, Aquanox 4630. They also have another formula
(Aquanox 4520) that I've not had a chance to use, that is supposed to be
better than the 4512P. You might want to give them a call...

-Steve Gregory-

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dan Mauro
Sent: Monday, November 06, 2006 9:56 AM
To: [log in to unmask]
Subject: [TN] Cleaning media for no clean paste

Folks,



I need to clean the residual residue left if any on boards processed
with no clean paste.

What should one use.  Any thoughts - is there a common chemical cleaner
that can penetrate under components.



Thanks in Advance

Dan


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



---------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Want to start your own business? Learn how on Yahoo! Small Business.

ATOM RSS1 RSS2